薄灰缝砌筑加气温凝土砌体力学性能试验研究
杨伟军,郏思文
(长沙理工大学,湖南长沙 410076)
摘要:加气混凝土材料作为能够满足节能65%要求的单一墙体材料,在应用中存在厚砂浆灰缝热桥作用的问题。研究表明,采
用薄层砂浆砌筑,减少了砂浆用量,砌体抗压强度随灰缝厚度的减小而提高,抗剪强度随灰缝厚度的减小而降低。
关键词:加气混凝土砌块;薄层砂浆;砌筑;抗压强度;抗剪强度
中图分类号:+2 文献标识码:B 文章编号:1001—702X(2011)01—0034—03
Experimental researchon mechanicalaeratedofconcrete masonrymortarthin th properties joint 1=.
YANG Weijun,JIA Siwen
(Changsha University of Science and Technology,Changsha 410076,Hunan,China)
Abstract:As the only wall material which can save 65% energy,aerated concrete has the problem of thermal bridge in thick
mortar joint during adoption of thin mortar joint can not only reduce the quantity mortar,butof improve the also reduce quantity canthe only not joint mortar thin of joint adoption mortar
compressive strength of the masonry and decrease its shear strength with the reduce of joint thickness. thickness. joint of reduce with the strength shear masonrythe its and decrease of pressive
K words:aerated concrete block;thin mol~arjoint;pressive strength;shear strength
表 1 试件的设计
目前我国加气混凝土砌块砌筑灰缝厚度大多为 10 15
film,灰缝对导热系数的影响很大,大大降低了墙体的热工性
能,此外,还加大了砂浆材料的用量,增加墙体的自重等。现
行欧洲国家砌块建筑普遍提倡使用薄灰缝砌筑技术,灰缝厚
度不大于mm,这不仅提高了砌体的热工性能,对力学性能 5 试验在长沙理工大学公路学院试验室的50t压力机上进
也产生了一定的影响【1I。而我们对不同灰缝厚度砌筑的加气行,砌体表面不够水平时在上承面上垫标准细砂参照 GBJ
混凝土砌块砌体的力学性能却不甚了解。现通过对采用加气 129—90《砌体基本力学性能试